This tests were made with GRP profiles rather GRP gratings. The flammability has to be agreed according the application. | Standard | Test method / remark | Country | Result |
|---|
| ÖNORM B 3800 | B1-Test/ phenolic resin | A | B1 Tr1 Q1 | | UNIFER E 10.02.977 | UNI 9177 classification | CH, I | 2A | | UNIFER E 10.02.977 | UNI 9174 burning heat FT | CH, I | 2A | | UNIFER E 10.02.977 | UNI 8457 KI FT | CH, I | 2A | | UNIFER E 10.02.977 | ISO 5660-1 heating energy | CH, I | see test report | | UNIFER E 10.02.977 | EN ISO 1716 heating value | CH, I | 7639 J/g | | DIN 53 438, part 2 | 5 mm | D | K 1/5 mm | | DIN 54837 | DIN 55 10 T2 | D | S4 SR2 ST2 | | DIN EN 13501 –1 | DIN EN ISO 9239 -1 | D EU | 9,9 kW/m2 / 195% min | | DIN EN 13501 –1 | DIN EN ISO 11925-2 | D EU | standards fulfilled | | DIN EN 13501 –1 | (≈DIN 4102-B1) | D EU | Bfl –s1 | | NFF16 -101 | NF X 70 -100 toxicity | F | F1/I.T.C.-Wert: 2,3 | | NFF16 -101 | NF X 10 -702 smoke | F | F1/I.T.C.-Wert: 2,3 | | NFF16 -101 | NF P 92-501 fire | F | M 2 | | BS 476: Part 7: 1997 | 8 mm | GB | class 2 | | BS 476: Part 7: 1997 | 3 mm | GB | class 2 | | UIC 564-2: 1994 | Annex 4 | H | fire C / smoke A | | NFPA 130 | ASTM E 662 smoke density | USA | see test report | | NFPA 130 | ASTM E 162 flame spread | USA | Is = 9,7 | | NFPA 255 | ASTM E-84-98 | USA | < 25, class A | | Code 95/28/EG: 1995 | Automobile Code, Burning speed 95/28/EG: 1995 | EU | standards fulfilled | | EN ISO 11925-2: 2002 | CEN/TS 45545-2: 2009 Ingnition | EU | standards fulfilled | | ISO 5660-1: 2002 | CEN/TS 45545-2: 2009 Heat release | EU | MAHRE 50,7 kW/m2 | | ISO 5658-2: 2006 | CEN/TS 45545-2: 2009 Flame psead | EU | CFE > 20 kW/m2 Qsb 8,13 MJ/m2
| | ISO 5659-2: 2007 | CEN/TS 45545-2: 2009 Smoke toxicity | EU | Ds (4) 89 VOF 4 95 CIT 4 min 0,01 CIT 8 min 0,02 | | ISO 4589-2 | Oxygen index by RT | EU | LOI 36,2% | | DIN EN 60695-11-10 | vertical test UL94 V | EU | V 0 |
|
|
|